ABSTRACT:
newlineIntroduction : Cobalt-chromium (Co-Cr) alloy is a commonly used material in
newlinedentistry due to its excellent mechanical properties and biocompatibility. The use
newlineof 3D printing technology for the fabrication of Co-Cr copings has increased in
newlinerecent years due to its high accuracy and efficiency. However, the bond strength
newlinebetween the Co-Cr copings and ceramic is crucial for the success of the
newlinerestoration.
newlineAim : The aim of this study was to evaluate the bond strength of Co-Cr copings
newlinefabricated using three different 3D printing machines, namely EOS, SHINING 3D,
newlineand OR LASER, to ceramic.
newlineMaterial and method : Eighteen Co-Cr copings were fabricated using DMLS
newlinetechnology and divided into three groups. Ceramic was applied to the copings
newlineusing a layering technique, and the bond strength was evaluated using a
newlineuniversal testing machine.
newlineResults : The results showed that the EOS group exhibited the highest mean
newlinedifferences among the three groups were statistically significant (p lt 0.05). The
newlinehigh bond strength values in the EOS and OR LASER groups could be attributed
newlineto the high-quality fabrication process and the excellent mechanical properties of
newlinethe Co-Cr alloy. The SHINING 3D group exhibited lower bond strength values in
newlineterms of incisors, which could be due to the use of a lower-power laser and less
newlineprecise control over the melting and solidification of the metal powder.
newlineConclusion : The results of this study suggest that the choice of 3D printing
newlinemachine can affect the bond strength between Co-Cr copings and ceramic.
newlineKeywords: Bond strength, DMLS, copings, cobalt chromium, LASER