Studies on the suitability of magnesium metal matrix composites for the application of air compressor piston

Abstract

Every industry is striving for finding a way to improve energy savings of a product, that directly affects their sustainability in the global market. One technique to conserve energy is the development of new materials with the sufficient strength. Magnesium metal matrix composites (MMC) have possessed a high specific strength and can fulfill the industrial expectations. Magnesium is a monolithic metal having a lesser density (1.74 g/cm3 ) than the other structural materials, such as aluminum (2.70g/cm3 ) and iron (7.87g/cm3 ). The present investigation involves the fabrication, characterization and application of magnesium metal matrix composites. In the view of application, an air compressor piston was considered. AZ91 magnesium alloy and tungsten carbide (WC) were used as the matrix and reinforcement materials, respectively. To produce the composites, a vacuum integrated stir casting setup was fabricated and employed. MMCs with 1.5 and 3.0 weight percentages (wt %) of WC (200 mesh in size) particulates, were fabricated (AZ91/1.5WC and AZ91/3.0WC). Surface characterization exposed the presence of inter-metallic phase, Mg17Al12 along with the primary phases. The captured scanning electron microscope (SEM) images of MMC samples exhibited the distribution of WC particles and the inter-metallic phase. Then the samples were subjected to solution heat treatment, ageing (T4 and T6) and cryogenic treatment separately. Conventionally followed thermal treatment parameters (solution heat treatment and aging temperatures, and times) of the matrix alloy were adopted to treat the MMCs also. Surface characterization revealed that T6 and cryogenic treatment enhanced the precipitation of hard Mg17Al12 phase in base alloy and its MMCs while the phase was dissolved in the matrix during T4 treatment.According to ASTM procedures, tensile, compression tests and bulk hardness measurement were conducted with the standard specimens. The tensile strength of the base alloy was reduced by 7 % and 10 % respectively with 1.5 wt % and 3.0 wt %

Description

Keywords

Citation

item.page.endorsement

item.page.review

item.page.supplemented

item.page.referenced