An Experimental Study On Strength And Durability Properties Of Ceramic Waste Concrete
Loading...
Date
item.page.authors
Journal Title
Journal ISSN
Volume Title
Publisher
Abstract
In the ceramic industry, approximately 15%-30% of total production waste is generated. At the moment, no form of this waste is recycled. A ceramic waste powder is also used as a binder with partial replacement of cement, which takes part of the reaction during hydration, and it also acts as a filler material. The mechanical properties of the concrete, such as its compressive, split tensile and flexural strengths, were measured in this study using ceramic waste powder in place of cement. Additionally, the size effect of the ceramic waste powder on the strength of the concrete was investigated. When exposed to acid, alkaline and temperature attacks, the performance of ceramic waste concrete on durability aspects was also investigated. Cement is substituted at various percentages 10%, 20%, 30%, 40%, and 50% by weight in concrete to test the effect on strength of replacing it with ceramic waste powder. To study the impact of particle size on ceramic waste powder, the powder is separated into two grades: one grade has particles less than 90 microns and the other has particles between 90 and 150 microns. Concrete mixtures for Ordinary Concrete M20, Standard Concrete M40, and High Strength Concrete M60 were developed for this study. According to the experimental findings, the introduction of Ceramic Waste Powder (CWP) in M20, M40, and M60 concrete results in a reduction in compressive strength, split tensile strength and flexural strength ranging from 10% to 50% when compared to Conventional concrete formulations. Significantly, within the spectrum of replacement percentages (10%, 20%, 30%, 40%, and 50%), the formulation with 10% CWP, featuring both particle sizes between 90-150 microns and less than 90 microns, exhibits enhanced strength. The compressive strength and weight of the specimens were found to be decreasing at a slower rate with age from the results of acid and alkaline attacks. Ceramic waste powder replacements between 10 and 20 percent were shown to work better than other replacements. Based on the results