Manufacturing and Synthesis and Characterization of Self Healing Nanocomposites
Loading...
Date
item.page.authors
Journal Title
Journal ISSN
Volume Title
Publisher
Abstract
The manufacturing and characterization processes are studied in depth for self-healing fiber reinforced composites and microcapsules. The composite structures fail due to internal cracks. These cracks are initiated due to continuous loading of structures. It is not possible to fill those cracks especially when the structures are at remote locations. Self-healing materials are designed and prepared to heal their cracks. The present work is about self-healing materials used for the fabrication of composites. It is expected that future applications are based on such advanced self-healing composite materials and thus it is needed to develop advanced self-healing composite structures. A brief review of self-healing techniques, self healing composite, synthesis of microcapsules as well as characterization of self healing capsules and composite material is discussed in the present investigation.
newlineThe internal cracks initiated by continuous stress on composite structures pose a significant challenge due to the difficulty of detection and repair, especially in remote locations. Self-healing composites offer a promising solution by autonomously repairing these cracks and preventing catastrophic failure. This research investigates the development and characterization of microcapsules and embedded in fibre matrix composite. The microcapsules loaded with healing agents were fabricated using a two-step encapsulation process and characterized for their internal and external morphology, as well as their performance. These microcapsules, constituting percentage weight of the composite material, were incorporated into the fabrication of self-healing composites, alongside glass fibers and epoxy resin. A comprehensive structural analysis was conducted to compare the performance of the self-healing composite with a normal composite without healing capabilities. Both materials underwent tensile, flexural and impact testing under identical conditions.