A Study on the Effect of Tool Profile and Groove Size In Friction Stir Welded Particulate Reinforced 6061 T6 Aluminium Alloy
Loading...
Date
item.page.authors
Journal Title
Journal ISSN
Volume Title
Publisher
Abstract
The main hindrances in the fabrication of the particulate reinforced aluminium matrix
newlinecomposites using friction stir welding (FSW) are: (i) inhomogeneity in particulate mixing with
newlinealuminium (Al) matrix, (ii) selection of tool profile, (iii) selection of welding parameters due
newlineto the mismatch in mechanical and thermal properties of the particulate and Al-matrix, and (iv)
newlinegroove dimensions, respectively. In particular, an optimum groove dimension plays a vital role
newlineto avoid the problem of agglomeration and inhomogeneous distribution of the reinforcement
newlinewithin the stirred region. The larger groove size requires larger mass of the reinforcement to
newlinefill the gap in the milled Al-matrix, while the smaller groove size leads to the inhomogeneous
newlinedistribution of the reinforcement within the stirred region. Therefore, the main objectives of
newlinethe dissertation are to study the effect of (i) simple tool profiles for producing the quality welds,
newline(ii) threaded tool in material mixing between the particulate (Al2O3) and (6061-T6) Al-matrix,
newlineand (iii) the optimization of the groove dimensions, respectively.
newlineA 3D coupled thermo-mechanical modelling using COMSOL Multiphysics software is
newlineused to investigate the effect of simple tool geometries on the material flow and the local heat
newlinegeneration at the tool pin profile/workpiece interface. The tool with four flats produces more
newlinelocal torque at the workpiece/tool interface and hence produces a good quality weld. The
newlinetapered threaded profile tool (TCT) produces the defect free and better mixing of the Al2O3
newlinepowder particles as compared to tool with four flats. The effect of groove dimension shows
newlinethat the nearly homogeneous/symmetric distribution of the reinforced Al2O3 powder particles
newlinein the 6061-T6 AA matrix have been observed in the case of groove width and depth of 2 mm
newlineeach. The level set (LS) physics coupled with the heat transfer physics to estimate the mixing
newlinebetween two fluids AA6061-T6 and Al2O3 confirms the better mixing in this combination. No
newlinedefects are observed for the