Experimental investigation on face milling of inconel 625 superalloy under cryogenic environments

Abstract

The machinability of Nickel based superalloy Inconel 625 is quite challenging due to increased heat generation at the cutting zone, which causes large heat accumulation at the tooltip, with dispersion of heat over the workpiece and the inability of the chips to deform during machining. In addition, a heavy thermo-mechanical load is experienced by the cutting inserts during the machining of nickel alloys. Therefore, this presents a scope to look out for alternative cooling techniques which must have low environmental footprint, economically feasible to use and the same time open up scope to increase machinability. Hence, well-designed lubrication and cooling techniques are required to reduce friction and lessen cutting temperature. Wet/flood coolant is often preferred by metal cutting industries for lubrication and cooling during metal cutting processes. However, it induces harmful effects on the machinist and the environment. Further, it also adds up to operational costs due to cleaning, disposal of chip, treatment and extraction of coolant. The problems faced by manufacturing industries during milling of nickel alloys are due to their poor thermal conductivity, work hardening behaviour and adhesion of chips onto the cutting tool. These unfavourable characteristics create excessive cutting tool wear and also produce an end product with a poor surface integrity index.In recent years, two cryogenic media, namely, liquid nitrogen and liquid carbon dioxide have been reported as promising lubricants or coolants in the metal cutting industries for the enhancement in machinability and surface integrity of Nickel-based superalloys. Variations in these coolants cooling capability and supply conditions into the machining zone, have great influence on the aforementioned characteristics. newline

Description

Keywords

Citation

item.page.endorsement

item.page.review

item.page.supplemented

item.page.referenced